Polimeri Europa Sinkral F 332 ABS Resin
Subcategory: ABS Polymer; Thermoplastic
Close Analogs: ISO 2580-ABS 1, MGN, 105-15-16-20
Material Notes: Sinkral F 332 is a general purpose injection molding grade which combines excellent thermal stability during processing with a good balance between flow and impact characteristics. Designation: Thermoplastic ISO 2580-ABS 1,MGN,105-15-16-20Applications: Suitable for use in a variety of industrial sectors, for the production of small household appliances and white goods, vacuum cleaners and telephones. Grade available in natural color only. Suitable masterbatches could be recommended for self-coloring. Information provided by Polimeri Europa
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Glow Wire Test
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|