Polimeri Europa SINKRAL B633/E ABS, Impact & Heat Stabilized Grade
Subcategory: ABS Polymer; Thermoplastic
Close Analogs: Polimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Key Words: Poly(Acrylonitrile Butadiene Styrene)
Material Notes: Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,EG,105-04-25-20 High impact extrusion grade with excellent stiffness, good processability and high thermal stability. Applications: Extrusion of sheets for industrial packaging, suitcases, refrigerator. Unfilled. Suitable for Profile Extrusion, Sheet Extrusion, Blow Molding, Thermoforming. Supplied as pellets. ISO data. Information provided by Enichem
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Glass Temperature
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|