Polimeri Europa SINKRAL C142/V4 ABS, Heat Stabilized, 17% Glass Fiber
Subcategory: ABS Polymer; Thermoplastic; Polymer
Close Analogs: Polimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Key Words: Poly(Acrylonitrile Butadiene Styrene)
Material Notes: Symbol according to ISO 1043-1-2: ABS (GF) Grade designation according to ISO 2580-ABS 1,MG,105-08-09-35,GF15 17% glass fibre reinforced injection moulding standard grade, with good impact resistance, high stiffness and very good flow. Main applications: teletronics (internal parts for fax-machines, video cassette recorders) and automotive (grilles). Filled. Suitable for Injection Molding. Supplied as pellets. Contains lubricant and release agent. ISO data. Information provided by Enichem
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Melt Flow
- Electrical Resistivity
- Surface Resistance
- Dielectric Strength
- Comparative Tracking Index
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|