Polimeri Europa SINKRAL L320 ABS
Subcategory: ABS Polymer; Thermoplastic
Close Analogs: Polimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Key Words: Poly(Acrylonitrile Butadiene Styrene)
Material Notes: Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-16-25 General purpose, high flow injection moulding grade having good impact resistance coupled with an excellent gloss. Normally used in the small appliance industry, as well as for vacuum cleaners, toys, telephones and consumer electronics. Unfilled. Suitable for Injection Molding. Supplied as pellets. Contains lubricant and release agent. ISO data except as noted. Information provided by Enichem
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Glass Temperature
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|