Ensinger Tecaform™ HPV 13 Acetal Homopolymer - Extruded Products
Subcategory: Acetal; Thermoplastic; Polymer; ; ; ; ; ; ; ; ;
Key Words: Polyoxymethylene (POM)
Material Notes: Tecaform™ HPV 13 is a brown homopolymer acetal with an internal PTFE lubricant. Its low coefficient of friction, excellent PV values, toughness, wear resistance, and machinability make it an exceptional material for use in many industrial and military components with moving parts. Additionally, Tecaform™ HPV 13 has superior chemical resistance and flexural fatigue properties, as well as low moisture absorption associated with acetal materials. Uses: Tecaform™ HPV 13's range of exceptional properties makes it an ideal engineering plastic for use in precision instruments and measuring devices, as well as in many critical components in the automotive, aviation, military, industrial, food processing machinery, business equipment, and specialty valve areas. Information supplied by Ensinger, Inc.
| Available Properties |
- Cost, 1 to 10 (Nylon = 2)
- Density
- Water Absorption
- Hardness, Rockwell R
- Tensile Strength at Break
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Machinability (1-10; 1 = easiest)
- Dimensional Stability (1-4; 4 = highest)
- Izod Impact, Notched
- Coefficient of Friction
- Coefficient of Friction, Static
- K (wear) Factor
- Limiting Pressure Velocity
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Brown
- FDA
- USDA
- NSF
- 3A-Dairy
- Canada AG
- USP Class VI available
- Acetaldehyde Aq. (40%)
- Acetamide Aq. (50%)
- Acetic Acid Aq. (10%)
- Acetone
- Alcohols, Aliphatic
- Allyl Alcohol
- Aluminum Chloride Aq. (10%)
- Aluminum Sulfate Aq. (10%)
- Ammonia Aq. (10%)
- Ammonia Gas
- Ammonium Carbonate Aq. (10%)
- Ammonium Chloride Aq. (10%)
- Ammonium Chloride Aq. (37%)
- Amyl Acetate
- Amyl Alcohol
- Aniline
- Barium Chloride Aq. (10%)
- Barium Sulfate Aq. (10%)
- Barium Sulfide Aq. (10%)
- Benzaldehyde
- Benzene
- Benzenesulfonic Acid
- Benzoic Acid Aq. (SAT)
- Benzyl Alcohol
- Beverages Aq. Alcoholic
- Beverages Aq. Carbonated
- Bitumen
- Bleaching Lye (10%)
- Bleaching Lye (100%)
- Boric Acid Aq. (10%)
- Bromine Aq. (30%)
- Bromine Liq.
- Butanol
- Butyl Acetate
- Butyl Phthalate
- Butylamine
- Butyric Acid Aq. (20%)
- Butyrolactone
- Calcium Chloride (in Alcohol) (20%)
- Calcium Chloride Aq. (10%)
- Calcium Hypochlorite
- Camphor
- Carbon Disulphide
- Carbon Tetrachloride
- Carbonic Acid Aq. (10%)
- Castor Oil
- Chloral Hydrate
- Chlorine Aq. (10%)
- Chlorine Gas (100%)
- Chloroacetic Acid Aq. (10%)
- Chlorobenzene
- Chloroform
- Chlorosulfonic Acid Aq. (10%)
- Chromic Acid Aq. (1%)
- Citric Acid Aq. (10%)
- Coconut Oil
- Creosote
- Cresols
- Cresylic Acid
- Cupric Chloride Aq. (10%)
- Cupric Sulfate Aq. (0.5%)
- Cupric Sulfate Aq. (10%)
- Cupric Sulfate Aq. (SAT)
- Cyclohexane
- Cyclohexanol
- Cyclohexanone
- Decalin
- Detergents, Organic
- Dibutylphthalate
- Dichlorodifluoro Methane
- Dichloroethylene
- Diesel Oil
- Diethyleneglycol Aq. (90%)
- Dimethyl Aniline
- Dimethyl Carbinol
- Dimethyl Formamide
- Dioxane
- Edible Oils
- Ethanol, Denatured (96%)
- Ether, Diethyl
- Ethyl Acetate
- Ethyl Chloride
- Ethylene Chloride
- Ethylene Chlorohydrin
- Ethylene Diamine
- Ethylene Dichloride
- Ethylene Glycol Aq. (96%)
- Ferric Chloride Aq. (10%)
- Ferric Chloride Aq. (5%)
- Ferrous Chloride Aq. (10%)
- Fluorine (Gas Wet)
- Fluorosilicic Acid Aq.
- Formaldehyde Aq. (10%)
- Formic Acid Aq. (10%)
- Formic Acid Aq. (3%)
- Freon 12 (Arcton 12)
- Fruit Juices (CONC)
- Furfural
- Gasoline
- Glycerine
- Heptane
- Hexane
- Hydrobromic Acid Aq. (10%)
- Hydrochloric Acid Aq. (0.4%)
- Hydrochloric Acid Aq. (10%)
- Hydrochloric Acid Aq. (2%)
- Hydrofluoric Acid Aq. (4%)
- Hydrogen Peroxide Aq. (0.5%)
- Hydrogen Peroxide Aq. (1%)
- Hydrogen Peroxide Aq. (3%)
- Hydrogen Sulfide Aq. (SAT)
- Hydrogenated Vegetable Oils
- Hydroquinone
- Iodine (3%)
- Iso octane
- Isopropyl alcohol
- Isopropyl Ether
- Lactic Acid Aq. (10%)
- Lactic Acid Aq. (90%)
- Lead Acetate Aq. (10%)
- Linseed Oil
- Lithium Bromide Aq. (50%)
- Lubricating Oils (Petroleum)
- Magnesium Chloride Aq. (10%)
- Magnesium Hydroxide Aq. (10%)
- Magnesium Sulfide Aq. (10%)
- Maleic Acid Aq. (CONC)
- Manganese Sulfate Aq. (10%)
- Mercuric Chloride Aq. (6%)
- Mercury
- Methanol
- Methyl Acetate
- Methyl Ethyl Ketone
- Methylene Chloride
- Milk
- Mineral Oils
- Naphthalene
- Nickel Sulfate Aq. (10%)
- Nitric Acid Aq. (0.1%)
- Nitric Acid Aq. (10%)
- Nitrobenzene
- Nitromethane
- Oleic Acid
- Oxalic Acid Aq. (10%)
- Ozone
- Paraffin
- Perchloric Acid Aq. (10%)
- Perchloroethylene
- Petroleum Ether
- Phenol (Molten)
- Phenol Aq. (6%)
- Phenol Aq. (75%)
- Phosphoric Acid Aq (0.3%)
- Phosphoric Acid Aq (3%)
- Phosphoric Acid Aq. (10%)
- Phthalic Acid Aq. (SAT)
- Potassium Acetate Aq. (50%)
- Potassium Bicarbonate Aq. (60%)
- Potassium Bromide Aq. (10%)
- Potassium Carbonate Aq. (60%)
- Potassium Chloride Aq. (90%)
- Potassium Dichromate Aq. (5%)
- Potassium Ferricyanide Aq. (30%)
- Potassium Ferrocyanide Aq. (30%)
- Potassium Hydroxide Aq. (10%)
- Potassium Hydroxide Aq. (50%)
- Potassium Nitrate Aq. (10%)
- Potassium Permanganate Aq. (1%)
- Potassium Sulfite Aq. (90%)
- Potassium Sulfite Aq. (CONC)
- Propane Gas
- Pyridine
- Resorcinol
- Salicylic Acid
- Silicone Fluids
- Silver Nitrate
- Soap Solutions
- Sodium (Molten)
- Sodium Acetate Aq. (60%)
- Sodium Benzoate Aq. (10%)
- Sodium Bicarbonate Aq. (50%)
- Sodium Bisulphite Aq. (10%)
- Sodium Bromide Aq. (10%)
- Sodium Carbonate Aq. (20%)
- Sodium Carbonate Aq. (50%)
- Sodium Chlorate Aq. (10%)
- Sodium Chloride Aq. (10%)
- Sodium Chloride Aq. (90%)
- Sodium Cyanide Aq. (10%)
- Sodium Hydroxide Aq. (10%)
- Sodium Hydroxide Aq. (50%)
- Sodium Hypochlorite 15% CI (Chlorine Bleach)
- Sodium Nitrate Aq. (50%)
- Sodium Perborate Aq. (10%)
- Sodium Phosphates Aq. (General)
- Sodium Silicate
- Sodium Sulfate Aq. (90%)
- Sodium Sulfide Aq. (90%)
- Sodium Thiosulfate Aq. (10%)
- Stannic Chloride Aq. (10%)
- Stearic Acid
- Styrene (Monomer)
- Sulfur
- Sulfur Dioxide (Dry Gas) (100%)
- Sulfuric Acid Aq. (2%)
- Sulfuric Acid Aq. (5%)
- Sulfuric Acid Conc.
- Sulfurous Acid Aq. (10%)
- Tallow
- Tar
- Tartaric Acid Aq.
- Tetrachlorethylene
- Tetrahydrofuran
- Tetralin
- Thionyl Chloride
- Thiophene
- Toluene
- Transformer Oil
- Trichlorethylene
- Triethanolamine
- Trisodium Phosphate Aq. (95%)
- Turpentine
- Urea
- Vaseline
- Vegetable Oils
- Vinegar
- Vinyl Chloride
- Water
- Wax (Molten)
- White Spirit
- Wines & Spirits
- Xylene
- Xylenol
- Zinc Chloride Aq. (10%)
- Zinc Oxide
- Zinc Sulfate Aq. (10%)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|