Ensinger ENSITEP® BT Polybutylene Terephthalate - Extruded Products
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic; Polymer;
Key Words: Polyester
Material Notes: ENSITEP BT is an unreinforced thermoplastic polyester derived from polybutylene terephthalate. Its excellent wear and impact resistance, low coefficient of friction, high flexural modulus, and superior dimensional stability make it a versatile material for designing mechanical and electro-mechanical parts. Because ENSITEP BT has no centerline porosity, the possibility of fluid absorption and leakage is virtually eliminated. Uses: ENSITEP's superior wear resistance and lack of centerline porosity give it an advantage over other materials for applications involving solvents, chemicals, and food products. ENSITEP is also used in water purification systems, printing equipment, textile components, food-handling equipment, and valves. Informatin supplied by Ensinger, Inc.
| Available Properties |
- Cost, 1 to 10 (Nylon = 2)
- Density
- Water Absorption
- Hardness, Rockwell M
- Tensile Strength at Break
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Machinability (1-10; 1 = easiest)
- Dimensional Stability (1-4; 4 = highest)
- Shear Modulus
- Izod Impact, Notched
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor, Low Frequency
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Black
- White
- UV Resistance (1-4; 4 = highest)
- Acetaldehyde Aq. (40%)
- Acetic Acid Aq. (10%)
- Acetone
- Alcohols, Aliphatic
- Aluminum Chloride Aq. (10%)
- Aluminum Sulfate Aq. (10%)
- Ammonia Aq. (10%)
- Ammonium Carbonate Aq. (10%)
- Ammonium Chloride Aq. (10%)
- Ammonium Chloride Aq. (37%)
- Amyl Acetate
- Amyl Alcohol
- Aniline
- Antimony Trichloride Aq. (10%)
- Barium Chloride Aq. (10%)
- Barium Sulfate Aq. (10%)
- Barium Sulfide Aq. (10%)
- Benzaldehyde
- Benzene
- Benzenesulfonic Acid
- Benzoic Acid Aq. (SAT)
- Benzyl Alcohol
- Beverages Aq. Alcoholic
- Bitumen
- Boric Acid Aq. (10%)
- Butanol
- Butyl Acetate
- Butyl Phthalate
- Butylene Glycol
- Butyric Acid Aq. (20%)
- Calcium Chloride Aq. (10%)
- Calcium Hypochlorite
- Carbon Disulphide
- Carbon Tetrachloride
- Carbonic Acid Aq. (10%)
- Chlorine Gas (100%)
- Chloroacetic Acid Aq. (10%)
- Chlorobenzene
- Chloroform
- Chlorosulfonic Acid Aq. (10%)
- Chromic Acid Aq. (1%)
- Citric Acid Aq. (10%)
- Citric Acid Aq. (SAT)
- Creosote
- Cresylic Acid
- Cupric Chloride Aq. (10%)
- Cyclohexane
- Cyclohexanone
- Detergents, Organic
- Dibutylphthalate
- Dichlorodifluoro Methane
- Diesel Oil
- Dimethyl Formamide
- Dioxane
- Ethanol, Denatured (96%)
- Ether, Diethyl
- Ethyl Acetate
- Ethyl Chloride
- Ethylene Chloride
- Ethylene Chlorohydrin
- Ethylene Dichloride
- Ethylene Glycol Aq. (96%)
- Ferric Chloride Aq. (10%)
- Ferric Chloride Aq. (5%)
- Ferric Chloride Aq. (SAT)
- Ferrous Chloride Aq. (10%)
- Fluorine (Gas Wet)
- Fluorosilicic Acid Aq.
- Formaldehyde Aq. (10%)
- Formic Acid Aq. (10%)
- Formic Acid Aq. (3%)
- Freon 12 (Arcton 12)
- Fruit Juices (CONC)
- Furfural
- Glycerine
- Heptane
- Hexane
- Hydrobromic Acid Aq. (10%)
- Hydrochloric Acid Aq. (0.4%)
- Hydrochloric Acid Aq. (10%)
- Hydrochloric Acid Aq. (2%)
- Hydrofluoric Acid Aq. (4%)
- Hydrogen Peroxide Aq. (0.5%)
- Hydrogen Peroxide Aq. (1%)
- Hydrogen Peroxide Aq. (3%)
- Hydrogen Sulfide Aq. (SAT)
- Iodine (3%)
- Iodine (in Alcohol)
- Iso octane
- Isopropyl alcohol
- Lactic Acid Aq. (10%)
- Lactic Acid Aq. (90%)
- Lead Acetate Aq. (10%)
- Linseed Oil
- Lubricating Oils (Petroleum)
- Magnesium Chloride Aq. (10%)
- Magnesium Hydroxide Aq. (10%)
- Maleic Acid Aq. (CONC)
- Mercury
- Methanol
- Methyl Acetate
- Methyl Ethyl Ketone
- Methylene Chloride
- Milk
- Mineral Oils
- Naphthalene
- Nickel Sulfate Aq. (10%)
- Nitric Acid Aq. (0.1%)
- Nitric Acid Aq. (10%)
- Nitrobenzene
- Oleic Acid
- Oxalic Acid Aq. (10%)
- Ozone
- Paraffin
- Perchloroethylene
- Petroleum Ether
- Phenol Aq. (6%)
- Phenol Aq. (75%)
- Phosphoric Acid Aq (0.3%)
- Phosphoric Acid Aq (3%)
- Phosphoric Acid Aq. (10%)
- Potassium Bicarbonate Aq. (60%)
- Potassium Bromide Aq. (10%)
- Potassium Carbonate Aq. (60%)
- Potassium Chloride Aq. (90%)
- Potassium Hydroxide Aq. (10%)
- Potassium Hydroxide Aq. (50%)
- Potassium Permanganate Aq. (1%)
- Potassium Sulfite Aq. (90%)
- Potassium Sulfite Aq. (CONC)
- Propane Gas
- Pyridine
- Silicone Fluids
- Soap Solutions
- Sodium Acetate Aq. (60%)
- Sodium Bicarbonate Aq. (50%)
- Sodium Bisulphite Aq. (10%)
- Sodium Carbonate Aq. (20%)
- Sodium Carbonate Aq. (50%)
- Sodium Chlorate Aq. (10%)
- Sodium Chloride Aq. (10%)
- Sodium Chloride Aq. (90%)
- Sodium Cyanide Aq. (10%)
- Sodium Hydroxide Aq. (10%)
- Sodium Hydroxide Aq. (50%)
- Sodium Hypochlorite 15% CI (Chlorine Bleach)
- Sodium Nitrate Aq. (50%)
- Sodium Perborate Aq. (10%)
- Sodium Phosphates Aq. (General)
- Sodium Silicate
- Sodium Sulfate Aq. (90%)
- Sodium Sulfide Aq. (90%)
- Sodium Thiosulfate Aq. (10%)
- Stannic Chloride Aq. (10%)
- Stearic Acid
- Styrene (Monomer)
- Sulfur
- Sulfur Dioxide (Dry Gas) (100%)
- Sulfuric Acid Aq. (2%)
- Sulfuric Acid Aq. (5%)
- Sulfuric Acid Conc.
- Sulfurous Acid Aq. (10%)
- Tar
- Tartaric Acid Aq.
- Tetrachlorethylene
- Tetrahydrofuran
- Toluene
- Transformer Oil
- Trichlorethylene
- Triethanolamine
- Trisodium Phosphate Aq. (95%)
- Turpentine
- Urea
- Vegetable Oils
- Vinegar
- Vinyl Chloride
- Water
- White Spirit
- Wines & Spirits
- Xylene
- Zinc Chloride Aq. (10%)
- Zinc Sulfate Aq. (10%)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|