Entec Hylac® HF224 ABS
Subcategory: ABS Polymer; Thermoplastic
Material Notes: Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families. Information provided by Entec.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Notched @ -40°C
- Volume Resistivity
- CTE, linear 68°F
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Moisture Content
- Injection Pressure
- Back Pressure
- Shot Size
- Screw Speed
- Holding Pressure
- Injection Rate
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|