Entec Hysun™ 383 ASA
Subcategory: ASA Polymer; Thermoplastic
Close Analogs: Discontinued
Material Notes: Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families. Information provided by Entec.
| Available Properties |
- Density
- Tensile Strength @ Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|