Engineered Plastics Corporation EPABS 54 ABS
Subcategory: ABS Polymer; Thermoplastic
Key Words: Poly(Acrylonitrile Butadiene Styrene)
Material Notes: Injection Grade Pellets. GMP # 002. Property values below represent typical values. Information provided by Engineered Plastics Corporation.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|