Engineered Plastics Corporation EP Alloy 510B PC/ABS Alloy
Subcategory: Polycarbonate; ABS Polymer; Thermoplastic
Key Words: Polycarbonate; Poly(Acrylonitrile Butadiene Styrene)
Material Notes: Gray. Stiff tough and excellent color stability. Used in housings for computers, printers, copiers and for auto parts such as air ducts and instrument panels. GMP # 002; Ford # WSS585. Property values below represent typical values; black, gray, ext/inj grades and FR/non FR grades are available and can be tailored to meet specific requirements. Information provided by Engineered Plastics Corporation.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|