EPMG "DVD" Demetalized Polycarbonate Regrind
Subcategory: Polycarbonate; Thermoplastic
Key Words: EPMG PC; EPMG, Inc.
Material Notes: 99% clear, balance color, black, and coated material. This high melt index polycarbonate (PC), originally used for compact discs, is ideally suited for blending with low melt index PC materials (from sheet or bottles) to produce injection molding resins. Through a series of steps, the aluminum and inks are removed from the compact disk to produce a clear regrind. Depending on the Grade, this clear product can be compounded to various color specifications. Information provided by EPMG, Inc.
| Available Properties |
- Density
- Apparent Bulk Density
- Melt Flow
|
|
|
|