e-polymers TEKASTER™ F615GFR, Flame Retardant, 30% Glass Reinforced PET
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic; Polymer
Key Words: Poly Ethylene Terephthalate
Material Notes: 30% Glass Fiber Reinforced, Flame Retardant Information provided by E-Polymers Co. Ltd.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Rockwell M
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dissipation Factor
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Oxygen Index
- Processing Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|