e-polymers TEKALOY™ G70A2, Impact Resistance, Easy Molding PC/ABS Alloy
Subcategory: Polycarbonate; ABS Polymer; Thermoplastic
Material Notes: Impact Resistance, Easy Molding Information provided by E-Polymers Co. Ltd.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
- Mold Temperature
|
|
|
|
| Property Data |