e-polymers TEKALOY™ T80GFR, Flame Retardant, 30% Glass Fiber Reinforced PBT/ABS Alloy
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); ABS Polymer; Thermoplastic; Polymer
Material Notes: 30% Glass Fiber reinforced, Flame Retardant Information provided by E-Polymers Co. Ltd.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|