Engineered Polymer Solutions PBT VM 450, 20% Mineral Filled
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic
Material Notes: Plate-able. Natural and colors available. Injection molding grade. Uses: Automotive, appliances Information provided by Engineered Polymer Solutions.
| Available Properties |
- Density
- Viscosity Measurement
- Linear Mold Shrinkage
- Tensile Strength @ Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Back Pressure
|
|
|
|