Protective Coating Co. PC-7® Epoxy Paste
Subcategory: Epoxy; Adhesive; Thermoset
Close Analogs: Eight epoxies from Protective Coating Co. are listed in MatWeb. Data provided by the manufacturer.
Key Words: PC Epoxy
Material Notes: PC-7® is a tough job Epoxy formulation developed for maximum bonding power. Components A (grey) and B (black), when mixed, react to form a bond of tremendous strength. PC-7® formulation provides extended working time, giving user ample time to complete larger jobs, reposition work or make changes. High wet grab or tack of PC-7® makes overhead and sidewall work easy without drip or sag. PC-7® demonstrates excellent chemical resistance to mild acids, caustics, detergents, gasoline, fuel oil, salt, and fresh water. PC-7® will not bond to wax paper, TEFLON®, polyethylene, and some soft plastics.
| Available Properties |
- Density
- Water Absorption
- Hardness, Shore D
- Elongation at Break
- Flexural Yield Strength
- Compressive Yield Strength
- Shear Strength
- Gardner Impact
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|