Protective Coating Co. PC-11® White Epoxy Paste
Subcategory: Epoxy; Adhesive; Thermoset
Close Analogs: Eight epoxies from Protective Coating Co. are listed in MatWeb. Data provided by the manufacturer.
Key Words: PC Epoxy
Material Notes: PC-11® is a Heavy Duty-white epoxy Paste formulated by the manufacturer of PC-7.® After mixing, PC-11® can be applied to a dry, wet or underwater surface and will cure to an off white color. PC-11® formulation provides working time of over 1/2 hour, giving user ample time to complete larger jobs, reposition work or make changes. PC-11® demonstrates excellent chemical resistance to mild acids, caustics, detergents, gasoline, fuel oil, salt and fresh water. PC-11® will not bond to TEFLON®, polyethylene, and some soft flexible plastics.
| Available Properties |
- Density
- Water Absorption
- Hardness, Shore D
- Elongation at Break
- Flexural Strength
- Compressive Strength
- Shear Strength
- Gardner Impact
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|