Protective Coating Co. PC-Woody® Epoxy Paste
Subcategory: Epoxy; Adhesive; Thermoset
Close Analogs: Eight epoxies from Protective Coating Co. are listed in MatWeb. Data provided by the manufacturer.
Key Words: PC Epoxy
Material Notes: PC-WOODY® is an epoxy paste formulated to replace missing and rotted wood with structural strength greater than most wood. Use for permanent repairs on all types of wood-exterior or interior. Unlike typical wood fillers, PC-WOODY® is a permanent wood repair product.
| Available Properties |
- Density
- Water Absorption
- Hardness, Shore D
- Elongation at Break
- Flexural Yield Strength
- Compressive Yield Strength
- Shear Strength
- Gardner Impact
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|