Protective Coating Co. PC-SuperEpoxy™ Translucent Epoxy Putty
Subcategory: Epoxy; Adhesive; Thermoset
Close Analogs: Eight epoxies from Protective Coating Co. are listed in MatWeb. Data provided by the manufacturer.
Key Words: PC Epoxy
Material Notes: PC-SUPEREPOXY™ is a non-drip, thixotropic, translucent paste with unlimited uses in bonding, sealing, and as a filler for most materials. Unlike conventional liquid epoxies, PC-SUPEREPOXY™ can be applied to both vertical and overhead surfaces without drip or sag. PC-SUPEREPOXY™ is non-conductive and demonstrates excellent resistance to most chemicals, salt water, gasoline, and fuel oil.
| Available Properties |
- Density
- Water Absorption
- Hardness, Shore D
- Elongation at Break
- Flexural Yield Strength
- Compressive Yield Strength
- Shear Strength
- Gardner Impact
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|