Equistar Alathon® ETP H4745 High Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer; Equistar High Density Polyethylene; Equistar Polyethylene
Key Words: HDPE
Material Notes: Applications ALATHON H 4745 is a new, multi-purpose, high-flow resin featuring enhanced cold temperature impact performance, enhanced processability and thermal stability for fast cycling and exhibits good color and organoleptic properties. Typical applications are cultured dairy containers, margarine containers, butter tubs and promotional drink cups. Freezer applications include ice cream, sherbet and other frozen dessert containers.
Certifications H 4745 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.
Processing Techniques Specific recommendations for processing H 4745 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.
| Available Properties |
- Density
- Melt Flow
- Spiral Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Yield
- 1% Secant Modulus
- 2% Secant Modulus
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|