Equistar Petrothene® LP510300 High Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer; Equistar High Density Polyethylene; Equistar Polyethylene
Key Words: HDPE
Material Notes:
Applications PETROTHENE LLP 5103-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good drawdown. It is recommended for merchandise bags, and multi-wall sack liners and barrier sheeting. It is also useful as a blend component for improved stiffness and machineability.
Certifications LP 5103-00 meets the requirements of Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.
Processing Techniques Specific recommendations for processing LP 5103-00 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.
The physical properties are typical values and are not to be construed as specific product limits. Film properties obtained on 1.25 mil film produced using a 2.2:1 blow-up ratio.
| Available Properties |
- Density
- Water Vapor Transmission
- Oxygen Transmission Rate
- Thickness
- Melt Flow
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Dart Drop Test
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|