Equistar Microthene® G MN72700 Low Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: LDPE
Material Notes:
General Description Microthene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique properties of a polyolefin resin with a small ground particle size. Contact your Equistar sales and/or technical service representative for more information and specific recommendations for your application.
Process Techniques The microfine size and irregular shape of Microthene G powders facilitate dispersibility with other components. Specific suggestions can be made only when equipment, materials, process parameters and conditions of use are known. Contact your Equistar technical representative for more information.
Regulatory Status Microthene powders comply with certain Food and Drug Administration regulations, which may or may not permit their contact with food. Specific limitations or conditions of use may apply. Contact your Equistar Regulatory Affairs representative for more information.
| Available Properties |
- Density
- Particle Mesh Size
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Melting Point
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|