Equistar Petrothene® PM92973 Linear Low Density Polyethylene Black Concentrate
Subcategory: Polyethylene; Thermoplastic; LLDPE; Equistar Wire and Cable Grade; Polymer; Equistar Linear Low Density Polyethylene
Key Words: LLDPE; Telecom/ Telecommunications; Black Concentrate; Power Cable
Material Notes: Applications PETROTHENE PM 92973 is a black concentrate formulated to be used with PETROTHENE GA 808-091, a natural LLDPE let-down resin, for use in the extrusion of communications and power cable jacketing. Antioxidant, to ensure long-term stability, and a processing aid have been added. This resin can be successfully used with LLDPE, MDPE, HDPE and PP resins.
Processing Techniques PM 92973 should be let down at a ratio of 14.4:1 to yield the optimum 2.6% final carbon black loading. PM 92973 is 6.5% of the final product.
| Available Properties |
- Density
- Carbon Black Loading
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|