Equistar Aquathene® AQ120000 Ethylene Vinylsilane Copolymer
Subcategory: Thermoplastic; Equistar Wire and Cable Grade
Key Words: Moisture Cure
Material Notes: Applications AQUATHENE AQ 120-000 is an ethylene vinylsilane copolymer designed for use in low voltage, power cable applications. This natural resin can be crosslinked, by exposure to moisture after extrusion with an appropriate catalyst.
Processing Techniques AQ 120-000 can be extruded using conventional extrusion equipment. For example, AQ 120-000 has been extruded successfully using a 2.5", 20:1 extruder equipped with a Maddock mixing screw under suggested temperature conditions.
Certification Crosslinking of the total system, AQ 120-000 and an appropriate crosslinking catalyst such as AQUATHENE CM 04482, occurs after the materials are mixed during extrusion and exposed to moisture. Crosslinking can be achieved by exposure to steam, immersion in hot water or storage at ambient conditions. The time required to achieve crosslinking depends on the catalyst masterbatch and temperature of the moisture. Because conditions can vary considerably, contact your Equistar sales representative for detailed recommendations. AQ 120-000 should be stored separately from the crosslinking catalyst masterbatch unitl extrusion. This resin can be stored in bulk for several months without special packaging and should not require drying prior to extrusion.
Physical Properties All properties determined from compression molded plaques. The values listed for physical electrical properties are nominal only and are subject to normal variations consistent with the test methods and/or variations found acceptable to the industry.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Break
- Elongation at Break
- Feed Temperature
- Zone 2
- Zone 3
- Zone 4-x
- Adapter Temperature
- Die Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|