Equistar Petrothene® GA837091 Medium Density Polyethylene
Subcategory: Ethylene Vinyl Acetate; Thermoplastic; Equistar Wire and Cable Grade
Key Words: MDPE; Fiber Optic/Coaxial General Purpose; Telecom/ Telecommunications; Jacketing
Material Notes: Applications PETROTHENE GA 837-091 is a broad molecular weight, medium density resin designed for use as a base resin in wire and cable jacketing. An antioxidant has been added to ensure thermal stability.
Processing Techniques GA 837-091, like other thermoplastic polyolefin compounds, can be extruded as wire and cable insulation using a conventional extruder. Below are suggested extrusion conditions for GA 837-091. These conditions are intended as general guidelines only and are not optimum values, since manufacturing conditions, such as extruder type and size, affect the processing of thermoplastic resins. For exact recommendations, contanct your Equistar sales representative.
Industry Specifications GA 837-091 meets the requirements of the following: ASTM D1248, Type 11, Category 4, Class A, Grade E9. Federal LP390C, Type 11, Class M, Category 4, Grade 2.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Dielectric Constant
- Dissipation Factor
- Brittleness Temperature
- Feed Temperature
- Zone 2
- Zone 3
- Zone 4-x
- Adapter Temperature
- Die Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|