Equistar Alathon® M4621 High Density Polyethylene
Subcategory: Polyethylene; HDPE; Polymer; Equistar High Density Polyethylene; Equistar Polyethylene
Key Words: HDPE
Material Notes: Applications ALATHON M 4621 is a copolymer that provides outstanding stress crack resistance and low temperature impact strength. Typical applications include small two-piece engine gas tanks, waste disposal drums, and specialty injection molded parts.
Certifications M 4621 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.
Processing Techniques Specific recommendations for processing M 4621 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.
| Available Properties |
- Density
- Melt Flow
- Spiral Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Yield
- 1% Secant Modulus
- 2% Secant Modulus
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|