Equistar Petrothene® NA271009 Medium Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; MDPE; Polymer; Equistar Polyethylene
Key Words: MDPE
Material Notes: Applications PETROTHENE NA 271-009 is a medium density polyethylene resin designed to overwrap film applications. NA 271-009 exhibits good film optics and high stiffness.
Certification NA 271-009 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.
Processing Techniques Specific recommendations for processing NA 271-009 can only be made when the processing conditions, equipment and end use are known. For further suggestions, contact your Equistar sales representative.
Physical Properties These are typical values and not to be construed as specific product limits. Film gauge: 1.25 mils.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Dart Drop Test
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|