Equistar Petrothene® NA336149 Low Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer; Equistar Low Density Polyethylene; Equistar Polyethylene
Key Words: LDPE
Material Notes: Applications PETROTHENE NA 336 is a homopolymer resin specifically engineered for garment film and dry cleaning bag applications. This resin is also suitable for any application requiring thin gauge film constructions. NA 336 is know for its consistency, exceptional drawdown and processability.
Certification NA 336 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.
Processing Techniques NA 336 is specifically designed to provide outstanding drawdown at maximum outputs. The melt strength properties of this resin result in excellent bubble stability. This resin can be processes over a wide range of temperatures; however, recommended conditions are melt temperatures between 300°-330°F and a blow-up ratio between 2.0-2.5:1. Using proper techniques and equipment, drawdown to 0.25 mil is feasible at commercial production rates. Specific recommendations for processing NA 336 can only be made when the processing conditions, equipment and end use are known. For further suggestions, contact your Equistar sales representative.
Physical Properties These are typical values and not to be construed as specific product limits. Data obtained from film produced in a 3.5"(89mm) blown film line, commercially available 8"(203 mm)die, 375°F(191°C) melt extrusion temperature, 2:1 BUR, 1.25 mil (32 micron)
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Dart Drop Test
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Vicat Softening Point
- Haze
- Gloss
- Melt Temperature
- Antiblock
- Slip
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|