Equistar Petrothene® NA443023 Blown Low Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer; Equistar Low Density Polyethylene; Equistar Polyethylene
Key Words: LDPE
Material Notes: Applications PETROTHENE NA 443 is a series of low density/EVA copolymer resins for high impact/high clarity packaging applications. NA 443 exhibits excellent processability and good balance of optics and strong heat sealing characteristics.
Certification NA 443 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1350. This regulation allows the use of this ethylene vinyl acetate copolymer "…in articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.
Processing Techniques NA 443 has excellent drawdown characteristics that yield outstanding output rates. Optimum properties are obtained over a broad range of extrusion conditions at melt temperatures between 330°-380°F melt temperatures and a blow-up ratio between 1.7-3.0:1. Using proper techniques and equipment, NA 443 can be drawn to 1.0 mil at commercial production rates. Specific recommendations for the processing of NA 442 can be made only when the end use application, required properties and the processing equipment are known. For exact recommendations, please contact your Equistar representative.
Physical Properties These are typical values and not to be construed as specific product limits. Data obtained from film produced in a 3.5"(89mm) blown film line, commercially available 8"(203 mm)die, 375°F(191°C) melt extrusion temperature, 2:1 BUR, 1.25 mil (32 micron) gauge, 0.025"die gap at 130 lb/hr.
| Available Properties |
- Density
- Vinyl Acetate Content
- Thickness
- Melt Flow
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Elmendorf Tear Strength MD
- Dart Drop Test
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Vicat Softening Point
- Haze
- Gloss
- Melt Temperature
- Antiblock
- Slip
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|