Equistar Petrothene® NA942094 Low Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer; Equistar Low Density Polyethylene; Equistar Polyethylene
Key Words: LDPE
Material Notes: Applications PETROTHENE NA 942 is a series of resins designed especially for heavy duty film applications, such as bags used to package fertilizer, peat moss, decorative stone, and agricultural and construction materials. NA 942 exhibits excellent impact properties and puncture resistance.
Certification NA 942 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.
Processing Techniques Generally recommended extrusion conditions include a melt temperature range of 330°430°F; a blow-up ratio range of 1.8-2.5:1. Drawdown to 2.0 mils is possible at commercial rates when proper extrusion techniques are used. Specific recommendations for processing NA 942 can be made only when the end use applications, required properties and processing equipment are known. For exact recommendations, contact your Equistar sales representative.
Physical Properties These are typical values and not to be construed as specific product limits. Data obtained from film produced in a 3.5"(89mm) blown film line, commercially available 8"(203 mm)die, 375°F(191°C) melt extrusion temperature, 2:1 BUR, 1.25 mil (32 micron) gauge, 0.025"die gap at 130 lb/hr.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Thickness
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Dart Drop Test
- Film Tensile Strength at Break, MD
- Brittleness Temperature
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|