Equistar Petrothene® NA960070 Low Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer; Equistar Low Density Polyethylene; Equistar Polyethylene
Key Words: LDPE
Material Notes: Applications PETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good uniformity, ease of processing and good tensile strength.
Certification The basic resin NA 960 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.
Processing Techniques Specific recommendations for processing NA 960 can only be made when the processing conditions, equipment and end use are known. For further suggestions, contact your Equistar sales representative.
Physical Properties These are typical values and not to be construed as specific product limits. Data obtained from film produced in
| Available Properties |
- Density
- Thickness
- Melt Flow
- Tensile Strength @ Break
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Elongation at Break
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Dart Drop Test
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Vicat Softening Point
- Melt Temperature
- Antiblock
- Slip
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|