Equistar Petrothene® NA963083 Low Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer; Equistar Low Density Polyethylene; Equistar Polyethylene
Key Words: LDPE
Material Notes: Applications PETROTHENE NA 963 is a series of resins formulated with special antiblock additive and designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 963 exhibits uniformity, ease of processing and good tensile strength.
Certification The basic resin NA 963 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.
Processing Techniques Generally recommended extrusion conditions include a melt temperature range of 310°350°F; a blow-up ratio range of 1.8-2.5:1. Drawdown to 1.0 mils is possible at commercial rates when proper extrusion techniques are used. Specific recommendations for processing NA 963 can be made only when the end use applications, required properties and processing equipment are known. For exact recommendations, contact your Equistar sales representative.
Physical Properties These are typical values and not to be construed as specific product limits. Data obtained from film produced in a 3.5" (98 mm)blown film line, commercially available 8"(203 mm) die, 350°F(177°C) melt extrusion temperature, 2:1 BUR, 1.25 mil(32 micron)gauge, 0.025" die gap at 150 lb/hr.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Dart Drop Test
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Vicat Softening Point
- Brittleness Temperature
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|