Equistar Petrothene® NA204000 Low Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer; Equistar Low Density Polyethylene; Equistar Polyethylene
Key Words: LDPE
Material Notes: Applications PETROTHENE NA 204-000 is a general-purpose resin recommended for intermediate and light-weight coating applications at high speeds. NA 204-000 can be drawn down to weights of 2.0 lb/ream at line speeds of 1200 ft/min. on a variety of substrates including paper, foil, cellophane, polyester film and other base stocks. NA 204-000 yields excellent adhesion and heat sealing characteristics and low neck-in. It is recommended for general-purpose flexible packaging, foil mounting, laminating and aseptic packaging.
Certification NA 204-000 meets requirements of the Food and Drug Administration regulations 21 CFR 177.1520 and 21 CFR 176.170. These regulations (respectively) allow for the use of the olefin polymer in "…articles or components of articles intended for use in contact with food; "or as components of the uncoated or coated food-contact surface of paper and paperboard intended for use in producing, manufacturing, packaging, processing, preparing, treating, packing, transporting or holding aqueous and fatty food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.
Processing Techniques The maximum recommended melt temperature for NA 204-000 is 625°F. More specific recommendations can be made only when the processing equipment, conditions and end use are known. For further suggestions, contact your Equistar sales representative.
Physical Properties These are typical values and not to be construed as specific product limits.
| Available Properties |
- Density
- Water Vapor Transmission
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Elongation at Break
- Flexural Stiffness
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|