Equistar Petrothene® NA214000 Low Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer; Equistar Low Density Polyethylene; Equistar Polyethylene
Key Words: LDPE
Material Notes: Applications PETROTHENE NA 214-000 is a low density polyethylene resin specifically designed for high speed, light weight, extrusion coating applications. This resin can be drawn down to a coating weight of three pounds per ream at line speeds exceeding 1,500 fpm with minimum neck-in and no edge weave. NA 214-000 can be used for applications including sugar pouches, industrial and multi-wall bags, treated and primed films and laminations.
Certification NA 214-000 meets requirements of the Food and Drug Administration regulations 21 CFR 177.1520 and 21 CFR 176.170. These regulations (respectively) allow for the use of the olefin polymer in "…articles or components of articles intended for use in contact with food; "or as components of the uncoated or coated food-contact surface of paper and paperboard intended for use in producing, manufacturing, packaging, processing, preparing, treating, packing, transporting or holding aqueous and fatty food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.
Processing Techniques A melt temperature of 590°-620°F is recommended for use in processing NA 214-000 in light-weight coating applications. Electrostatic, flame or chemical priming should be used to ensure good adhesion. The maximum melt temperature that is recommended for NA 214-000 is 625°F. For further suggestions, please contact your Equistar sales representative.
Physical Properties These are typical values and not to be construed as specific product limits.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Elongation at Break
- Flexural Stiffness
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|