Equistar Petrothene® NA216000 Low Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer; Equistar Low Density Polyethylene; Equistar Polyethylene
Key Words: LDPE
Material Notes: Applications PETROTHENE NA 216-000 is a general purpose, heavy and medium weight coating resin, capable of coating weights down to 7.0 lbs/ream at line speeds of 1200 ft/min. It can be applied to paper, foil, cellophane, polyester film, and other base stocks by the conventional extrusion coating process. Products made from materials coated with NA 216-000 include flexible packaging milk cartons, set-up cartons and food boards and other materials.
Certification NA 216-000 meets requirements of the Food and Drug Administration regulations 21 CFR 177.1520 and 21 CFR 176.170. These regulations (respectively) allow for the use of the olefin polymer in "…articles or components of articles intended for use in contact with food; "or as components of the uncoated or coated food-contact surface of paper and paperboard intended for use in producing, manufacturing, packaging, processing, preparing, treating, packing, transporting or holding aqueous and fatty food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.
Processing Techniques The maximum recommended melt temperature for NA 216-000 is 625°F. For further suggestions, contact your Equistar sales representative.
Physical Properties These are typical values and not to be construed as specific product limits.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Elongation at Break
- Flexural Stiffness
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|