Equistar Alathon® L5332CP High Density Polyethylene

 

Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer; Equistar High Density Polyethylene; Equistar Polyethylene

Material Notes:
Applications
ALATHON L 5332CP, formerly known as LYHD 048, is designed to meet the requirements of AAHTO M294 stress crack resistance. It exhibits excellent processing stability and high crush resistance. Typical applications include corrugated pipe, conduit and profile extruded applications. L 5332CP conforms to ASTM D 3350 cell classification. NCTL > 24 hrs per AASHTO M294.

Certification
L 5332CP meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

Processing
Specific recommendations for processing L 5332CP can only be made when the processing conditions, equipment and end use are known.

Available Properties
  • Density
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength @ Break
  • Tensile Strength @ Yield
  • Elongation at Break
  • Elongation at Yield
  • 1% Secant Modulus
  • Tensile Impact
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Vicat Softening Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。