Equistar Aquathene® FR409800 Polyethylene Wire and Cable Compound
Subcategory: Polyethylene; Thermoset; Equistar Wire and Cable Grade; Polymer
Key Words: Colorable Flame Retardant Masterbatch; Power Cable; Moisture Cure
Material Notes: Applications AQUATHENE FR 4098-00 is a colorable flame retardant masterbatch designed specifically for moisture cure applications. When FR 4098-00 is combined with AQ 120-000 and CM 04482 in the correct ratio this formulation is suitable for use in 600-V power cable and control cable applications where UL44 horizontal flame rating and 90°C service in wet locations are required. When melt blended using 30 wt.% FR 4098-00, 5 wt.% CM 04482 and 65 wt.% AQ 120-000, this formulation is designed to meet the following UL requirements: SIS, XHHW, XHHW-2, RHH, RHW, and RHW-2.
Processing The moisture curable system of FR 4098-00, CM 04882 and AQ 120-000 can be extruded as wires and cable insulation using a conventional extruder. The total system, FR 4098-00, CM 04482 and AQ 120-000, crosslinks after the materials are mixed during extrusion and subsequently exposed to moisture. Crosslinking can be achieved by exposure to steam, immersion in water or storage at ambient conditions. Since cure time varies considerable with environmental conditions and cable constructions, contact your Equistar sales representative for detailed cure conditions.
| Available Properties |
- Density
- Melt Flow
- Feed Temperature
- Zone 2
- Zone 3
- Zone 4-x
- Adapter Temperature
- Die Temperature
- Wire Preheat Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|