Equistar Petrothene® GA616050 Linear Low Density Polyethylene

 

Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer; Equistar Linear Low Density Polyethylene; Equistar Polyethylene

Key Words: LLDPE

Material Notes:
Applications
PETROTHENE GA 616-050 is a linear low density polyethylene resin which can be dry blended with low density polyethylene coating resins to produce linear low extrusion coatings. LDPE grade NA 204-000 (0.918 density, 7.0 melt index) is the preferred low density polyethylene resin for this blend.

Processing Techniques
Specific recommendations for processing GA 616-050 can only be made when the processing conditions, equipment and end use are known. The maximum recommended melt temperature for GA 616-050 blended with LDPE is 625°F. Suggested blend ratios can be obtained by contacting your Equistar sales representative.

Available Properties
  • Density
  • Melt Index of Compound
  • Hardness, Shore D
  • Tensile Strength @ Break
  • Elongation at Break
  • Flexural Stiffness
  • Vicat Softening Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。