Equistar Alathon® L5876 High Density Polyethylene, Blow Molding Grade
Subcategory: Polyethylene; HDPE; Equistar High Density Polyethylene; Equistar Polyethylene
Material Notes: ALATHON L5876 is designed for injection blow molding and extrusion blow molding applications where higher gloss than standard grades is required. Regulatory Status: L5876 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food. " Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Specific recommendations for processing L5876 can only be made when the processing conditions, equipment and end use are known. For further suggestions please contact your Equistar sales representative.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Tensile Impact
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|