Equistar Alathon® L5005V High Density Polyethylene, HMW Film Grade
Subcategory: Polyethylene; HDPE; Equistar High Density Polyethylene; Equistar Polyethylene
Material Notes: ALATHON L5005V is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typical applications include merchandise bags, grocery sacks, trash can liners, produce bags and roll stock. Materials of animal origin are not used as plasticizers, additives, or raw materials in L5005V. Regulatory Status: L5005V meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food. " Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Specific recommendations for processing L5005V can only be made when the processing conditions, equipment and end use are known. For further suggestions please contact your Equistar sales representative.
| Available Properties |
- Density
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Dart Drop Total Energy
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Melt Temperature
- Die Opening
- Blow-up Ratio (BUR)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|