Equistar Petrothene® LP540200 High Density Polyethylene, Film Extrusion Grade
Subcategory: Polyethylene; HDPE; Equistar High Density Polyethylene; Equistar Polyethylene
Material Notes: PETROTHENE LP540200 is a copolymer resin designed for blown film applications. This resin offers high ESCR, stiffness, excellent appearance and bubble stability. LP540200 is recommended for high strength multi-wall sack liners and barrier sheeting. It is also useful as a blend component for improved stiffness and machinability.Regulatory Status: LP540200 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.
| Available Properties |
- Density
- Water Vapor Transmission
- Oxygen Transmission Rate
- ESCR 100% Igepal®
- Thickness
- Melt Flow
- Hardness, Shore D
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Tensile Strength, Yield
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Dart Drop
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
- Melt Temperature
- Die Opening
- Blow-up Ratio (BUR)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|