Equistar Alathon® M4855 High Density Polyethylene, Injection Molding Grade

 

Subcategory: Polyethylene; HDPE; Equistar High Density Polyethylene; Equistar Polyethylene

Material Notes:
ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 are consumer durables and 35, 65, and 95-gallon refuse carts.

Regulatory Status: Alathon M4855 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.

Specific recommendations for processing M4855 can only be made when the processing conditions, equipment and end use application are known.

Available Properties
  • Density
  • Bulk Density
  • Melt Flow
  • Spiral Flow
  • Tensile Strength @ Break
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Izod Impact, Notched
  • Izod Impact, Unnotched @ -18°C
  • Melting Point
  • Crystallization Temperature
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Vicat Softening Point
  • Brittleness Temperature
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。