Equistar Alathon® H6017 High Density Polyethylene, Injection Molding Grade
Subcategory: Polyethylene; HDPE; Equistar High Density Polyethylene; Equistar Polyethylene
Material Notes: ALATHON H6017 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include housewares, caps, closures and various food containers.Regulatory Status: H6017 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Specific recommendations for processing H6017 can only be made when the processing conditions, equipment and end use application are known.
| Available Properties |
- Density
- Bulk Density
- Melt Flow
- Spiral Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Unnotched @ -18°C
- Melting Point
- Crystallization Temperature
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|