Equistar Alathon® L4904 High Density Polyethylene, Pipe and Sheet Extrusion Grade
Subcategory: Polyethylene; HDPE; Equistar High Density Polyethylene; Equistar Polyethylene
Material Notes: Alathon L4904 is a bimodal, high molecular weight, high density polyethylene resin with excellent processability characteristics that meet the high performance requirements of demanding pressure pipe applications including gas distribution, industrial piping, gas gathering, municipal water service lines and sewers. L4904 is designed specifically to provide superb resistance to pipe failure by rapid crack propagation and slow crack growth mechanisms. When L4904 is compounded with an Equistar approved black at the correct loading (see page 2) this formula meets the following standards.- Plastics Pipe Institute (PPI) PE 4710.
- PE 100 per PPI TR-4.
- ASTM D 3350 Cell Classification 445574C and 445576C.
- Chemical Resistance per ASTM D 2513
- NSF Standard 14 and Standard 61 for Potable Water Pipe and Fittings.
| Available Properties |
- Density
- PENT
- Melt Flow
- Tensile Strength @ Break
- Tensile Strength, Yield
- Elongation at Break
- Creep Strength
- 2% Secant Modulus
- Hydrostatic Design Basis @ 73°F
- Brittleness Temperature
- DSC Induction Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|