Equistar Alathon® L5008HP High Density Polyethylene, Pressure Pipe Extrusion Grade
Subcategory: Polyethylene; HDPE; Equistar High Density Polyethylene; Equistar Polyethylene
Material Notes: ALATHON L5008HP is a bimodal, high molecular weight, high density polyethylene resin with excellent processability designed to meet the high performance requirements of pressure pipe applications including gas distribution, industrial piping, gas gathering, municipal water service lines and sewer lines. When L5008HP is compounded with an Equistar approved black concentrate this formula meets the following standards.- Plastics Pipe Institute (PPI) PE 4710 per ASTM D 3350-06
- Plastics Pipe Institute (PPI) PE 3408 per ASTM D 3350-02a
- NSF Standard 14 and Standard 61 for Potable Water Pipe and Fittings.
- ASTM D 3350 Cell Classification 445574C.
- Chemical Resistance per ASTM D 2513-01a, Section 5.4.
| Available Properties |
- Density
- PENT
- Melt Flow
- Tensile Strength @ Break
- Tensile Strength, Yield
- Elongation at Break
- 2% Secant Modulus
- Hydrostatic Design Basis @ 73°F
- Deflection Temperature at 0.46 MPa (66 psi)
- DSC Induction Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|