Equistar Lupolen® 5261 Z Q 456 B High Density Polyethylene, Pipe and Sheet Extrusion Grade
Subcategory: Polyethylene; HDPE; Equistar High Density Polyethylene; Equistar Polyethylene
Material Notes: Lupolen 5261 Z Q 456 B is a high density polyethylene (HDPE) with high melt viscosity for ram extrusion of peroxide crosslinked pipes (PE-Xa). The product is supplied as a nominal 20 mesh (840 um) powder. It is not intended for medical or pharmaceutical applications. Processing Method: Extrusion Pipe, Sheet and Semi Finished Products. Physical Form: Powder. Typical Customer Applications: Plumbing, Heating and Cooling.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Melting Point
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|