Equistar Petrothene® GA564189 Linear Low Density Polyethylene, Injection Molding Grade
Subcategory: Polyethylene; LLDPE; Equistar Linear Low Density Polyethylene; Equistar Polyethylene
Material Notes: PETROTHENE GA564189 exhibits good stiffness and low temperature toughness. Typical applications include trash cans, industrial containers, housewares and toys. Regulatory Status: GA564189 meets the requirements of the Food and Drug Administration 21 CFR 177.1520. This regulation allows the use of this olefin polymer in” …articles or components or articles intended for use in contact with food.” Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Specific recommendations for processing GA564189 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.
| Available Properties |
- Density
- Melt Flow
- Spiral Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength, Yield
- Elongation at Yield
- 1% Secant Modulus
- 2% Secant Modulus
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|