Equistar Petrothene® GA694189 Linear Low Density Polyethylene, Injection Molding Grade
Subcategory: Polyethylene; LLDPE; Equistar Linear Low Density Polyethylene; Equistar Polyethylene
Material Notes: PETROTHENE GA694189 is a pelletized LLDPE copolymer resin for injection molding. Typical applications include lids and thin-walled items that require high flow and short cycle times. GA694189 exhibits excellent flow, warp resistance and surface appearance. Specific recommendations for processing GA694189 can only be made when the processing conditions, equipment and end use are known. Contact your Equistar sales representative for more information.
| Available Properties |
- Density
- Melt Flow
- Spiral Flow
- Hardness, Shore D
- Tensile Strength @ Break
- 1% Secant Modulus
- 2% Secant Modulus
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|