Equistar Petrothene® NA967000 Low Density Polyethylene, Film Extrusion Grade
Subcategory: Polyethylene; LDPE; Equistar Low Density Polyethylene; Equistar Polyethylene
Material Notes: Petrothene NA967000 is a low density polyethylene resin designed for blown film, general purpose and industrial packaging applications. NA967000 exhibits good processing characteristics and impact strength.Regulatory Status: NA967000 meets the requirements of the Food and Drug Administration, 21 CFR 177.1520. This regulation allows the use of this olefin polymer "...in articles or components of articles intended for use in contact with food," except in cooking applications. Specific limitations or conditions of use do apply. Contact your Equistar sales representative for more information. Specific recommendations for processing NA967000 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Elongation at Break
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Dart Drop
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Vicat Softening Point
- Brittleness Temperature
- Melt Temperature
- Die Opening
- Blow-up Ratio (BUR)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|