Equistar Purell® PE3220D Low Density Polyethylene, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding
Subcategory: Polyethylene; LDPE; Equistar Low Density Polyethylene; Equistar Polyethylene; Blow Molding
Material Notes: Purell PE 3220 D is a low density polyethylene with high rigidity and good chemical resistance. It is delivered in pellet form. Target markets are packaging of pharmaceuticals in the small blow molding market. Regulatory Status: Purell PE 3220 D meets the requirements of the Food and Drug Administration, Code of Federal Regulations, 21CFR Section 177.1520. This regulation allows the use of this olefin polymer in "articles or components of articles intended for use in contact with food." Contact your Equistar sales representative for more information regarding the suitability of specific products for specific applications. Specific recommendations for processing Purell PE 3220 D can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Break
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|